Bearing Adapter - Ductile Cast Iron-50
Type: Other | Material: Ductile cast iron -50 GOST 7293-85 | Dimensions (L x W x H) (mm): 253mm X230mmX130mm | Place of Origin: Shandong China (Mainland) |
Brand Name: CRV | Model Number: Ductile Cast Iron-50 | Ductile casr Iron-50: Railway Part | Ductile Cast Iron: Ductile Cast Steel |
We can produce Railway Ductile Casting Iron part and Casting Steel Part according to Russia GOST Standard or ASTM Standard, also produce Cast Steel Part for mining machinery and automobile industry.
Russia Bearing Adapter 4536-07. 00.00.001, ductile cast iron-50
1.Dimension:253 X230X130 Weight:18.9Kg
2. Material: Ductile cast iron -50 GOST 7293-85
Correspond between T500-7 and QT600-3 of GB/T1348-2009
3.Circumferential machining
4. Heat Treatment Method:High Frequency Quenching Surface Hardness :350-450HB
5. (GB11)Accuracy of casting: 11T-0-0-10 GOST P53464-2009
6. Mass content of the elements:
C | Si | Mn | P | S | Cr | Cu | Ni | Mg | Ti | Mo | Al | V |
3.6-3.8 | 2.4-2.6 | 0.2-0.4 | ≤0.03 | ≤≤0.02 | ≤0.05 | ≤0.4 | ≤0.05 | 0.04-0.06 | ≤0.04 | ≤0.02 | ≤0.04 | ≤0.05 |
7. Mechanical Property requests:
Ultimate tensile strength MPa | Yield strength MPa | Relative elongation | Hardness HB | Surface Hardness HB | Impact Strength KCV at + 20°C KJ/M² | KJ/M2 Impact strength KCV -60°C KJ/M² |
≥552 | ≥379 | ≥6 | 187-255 | 350-450 | 100-120 | 65-75 |
9. Molding Method: Resin Sand Metal Hand Molding
10. Melting Method: Medium Frequency Induction Furnace Melting
11. Spheroidization Treatment Method:
(1) Strictly Control the Oven Material, avoid to form strongly carbonization elements such
as Cr.,V. , Mo etc. Mn remove low limit, prevent from free cementite as- cast state
(2)Amount of Preparation, (0.5--0.7)%, one hand prevent from Carbonization , other hand prevent from forming amount of ferrite.
(3) Add appropriate amount of Cu stable pearlite, (0.3-0.4)%
12. Heart Treatment Method: High Frequency Quenching(The aim is getting martensite structure from casting surface, can improve abrasion resistance of
casting surface, same time can keep cast heart in good formability and tolerance)
Adopting Frequency 10KHz---2MHz Power Density 10.9—18.6W/mm2,Medium:Water Quenching Temperature:(900-925°C)
13. Chemical Elements Test: Arrange chemical elements test through direct-reading spectrometer(GOST 7293-85)
C | Si | Mn | P | S | Cu | Cr | Ni | Mg |
3.63 | 2.52 | 0.31 | 0.025 | 0.016 | 0.28 | 0.002 | 0.001 | 0.045 |
14. Mechanical Property Test(GOST 7293-85)
Ultimate Tensile strength MPa | Yield Strength MPa | Relative elongation | Hardness HB | Surface Hardness HB | Impact Strength KCV at + 20°C KJ/M² | KJ/M2 Impact strength KCV -60°C KJ/M² |
565 | 383 | 7 | 208 | 412 | 115 | 69 |
Packaging Detail:Wood packing, 2piec in a wood box 0.018CBM |